Fire Retardant 1.5g/cm3 PVC Compound For Cable Insulation Sheathing
Contact Person : Ariel Zhang
Phone Number : +86 13580878248
WhatsApp : +8613580878248
Minimum Order Quantity : | 1ton | Price : | 800-1200/Ton |
---|---|---|---|
Packaging Details : | 900kg per jumbo bag /25kgs per little bag | Delivery Time : | 1-2 weeks |
Payment Terms : | L/C, T/T | Supply Ability : | 800 tons per month |
Place of Origin: | China | Brand Name: | Anan |
---|---|---|---|
Certification: | Reach,Rohs,UL,ISO 9001 | Model Number: | PVC Compound |
Detail Information |
|||
Color: | Customized | Material: | Virgin Pvc Resin,Environment-friendly PVC |
---|---|---|---|
Application: | Cable Wire Sheath | Appearance: | Granule,granules/pellet |
Sample: | For Free | Operation: | Extrusion Or Injection Process |
Density: | 1.5cm3 | Hardness: | 88A |
High Light: | 88A PVC Recycled Granules,1.5cm3 PVC Recycled Granules,Cable Wire PVC Compound |
Product Description
Pvc Material Pvc Compound Pvc Granule For Cable Wire
Product Introduction:
PVC cable material is based on polyvinyl chloride resin, added stabilizer, dioctyl phthalate, diisodecyl phthalate, dioctyl terephthalate, trioctyl trimellitate, etc.
Plasticizers and inorganic fillers such as calcium carbonate, additives, lubricants and other additives are prepared by mixing, kneading and extruding particles.
PVC material is polyvinyl chloride. It is one of the largest plastic products in the world. It is cheap and widely used. Polyvinyl chloride resin is white or light yellow powder.
It cannot be used alone and must be modified. PVC is a white powder with an amorphous structure, with a small degree of branching, and poor stability to light and heat.
Different additives can be added according to different purposes, and PVC plastics can present different physical and mechanical properties.
Technical Data:
Items | Unit | Typical Value | Testing Method | ||
70 ℃ PVC Cable Compound | 105 ℃ PVC Cable Compound | 105 ℃ Irradiated crosslinked FR PVC Compound | |||
Tensile Strength | Mpa | 11 | 11 | 12 | GB/T 1040.3-2006 |
Elongation at Break | % | 180 | 180 | 180 | |
Heat Aging | |||||
Testing Termperature | ℃ | 100 | 135 | 135 | GB/T 8815-2008 |
Testing Time | h | 168 | 168 | 168 | |
Variation at tensile strength | % | 20 | 20 | 20 | |
Variation at elongation | % | -15 | -15 | -15 | |
Low Temperature Brittleness | ℃ | -20 | -20 | -20 | GB/T 5470-2008 |
Oxygen Index | / | ≥23 | ≥23 | ≥28 | GB/T 2406.2-2008 |
Density | g/cm3 | 1.42 | 1.42 | 1.42 | GB/T 1033.1-2008 |
Hardness | Shore A | 70-96 | 70-96 | 70-96 | GB/T 2411-2008 |
Product Show: